Effect of electric current on phase frormation in tungsten monocarbide in the process of electro consolidation of nano powders.
Opis bibliograficzny
Szczegóły publikacji
Streszczenia
The tendency of content gain of tungsten semi carbide (di-tungsten carbide) W2C after rapid sintering of compact ceramic structures on the base of tungsten carbide (monocarbide) WC from nano powders technology-based on electro consolidation under pressure is been considered. The issues of the genesis of W2C expansion in new technologies for producing nanostructured single-phase WC ceramics have been formulated and explained. The mechanisms of W2C carbide formation have been examined. By completely eliminating W2C, a single-phase tungsten monocarbide was obtained, with a fracture toughness of 10 MPa·m1/2 and a hardness of HV10=31GPa.
Open Access
Linki zewnętrzne
Identyfikatory
Metryki
Eksport cytowania
Wsparcie dla menedżerów bibliografii:
Ta strona wspiera automatyczny import do Zotero, Mendeley i EndNote. Użytkownicy z zainstalowanym rozszerzeniem przeglądarki mogą zapisać tę publikację jednym kliknięciem - ikona pojawi się automatycznie w pasku narzędzi przeglądarki.
Informacje dodatkowe
Rekord utworzony: | 9 lipca 2024 10:51 |
---|---|
Ostatnia aktualizacja: | 9 lipca 2024 10:51 |